Technical FAQ

Technical FAQ

Home | Technical FAQ

The questions below cover selection, systems, application and document requests most often raised. Where a specific parameter is involved, the technical data sheet governs; the contact page can also advise on selection for a given service condition.

Selection and systems

How is the right model chosen?
State the substrate, the surface preparation grade, the service environment (atmospheric exposure, immersion, buried service or the medium contacted) and the design dry film thickness; candidate models and the order of coats are then proposed as a system.
How are primer, intermediate and topcoat combined?
Follow the system requirements: adjacent coats must be compatible, and different systems should not be mixed. Each model page lists the coating position and the systems the model belongs to.
How are industrial and marine coatings divided?
The range is divided into two lines: industrial coatings cover steel structures, tanks and pipework, concrete, power and renewables; marine coatings cover hull antifouling, ballast and void spaces, waterline and underwater areas.
Can a single model be purchased and combined independently?
Yes. Compatibility, however, is governed by the technical data: select adjacent coats from the system table to avoid inter-coat adhesion problems caused by incompatible systems.

Documents, quantities and quotation

What documentation is available?
Technical data sheets (TDS) and safety data sheets (SDS), available on request by model.
What governs the parameters shown here?
The technical data sheet governs. Parameters shown on model pages are taken from the technical data; where the data gives no value the page says available on request — nothing is inferred or filled in.
How is consumption calculated?
Theoretical spreading rate (m²/L) = volume solids × 10 ÷ design dry film thickness (µm). Practical consumption also allows for surface roughness and application losses; this site can carry out the calculation.
How is an order placed, and who quotes?
Use the contact page for technical enquiries: state the grade, the quantity and the destination, and a quotation follows per grade, together with the TDS and SDS.

Application and site issues

How is the surface preparation grade determined?
For steel, ISO 8501-1 blast cleaning grades Sa2½ and Sa3 are common, together with hand and power tool grades St2 and St3.The higher the grade, the better adhesion and durability; the grade to use is as required by the data sheet of the model selected.
What are the application conditions?
Steel temperature must be at least 3 °C above dew point before application; relative humidity and the minimum application temperature follow the technical data. Application stops if the surface carries condensation, frost or moisture.
How are wet and dry film thickness converted?
Wet film thickness (µm) = design dry film thickness ÷ volume solids × 100. Wet film gauging controls application on site, dry film gauging verifies the cured film, and acceptance follows the film thickness range in the technical data.
How is the overcoating interval controlled?
Minimum and maximum overcoating intervals are set by the technical data. Beyond the maximum interval, sweeping or surface preparation is required as specified, to secure inter-coat adhesion; too short an interval can cause lifting or solvent retention.
How are pinholing, sagging or blistering investigated?
They are usually linked to inadequate surface preparation, too low an application viscosity, too thick a single coat, high ambient humidity or an unsuitable thinner. Check the application record and the ambient conditions first, then work through the technical data item by item; take samples for re-testing where necessary.
What matters when overcoating a zinc-rich primer?
Zinc salts (white rust) form readily on a zinc-rich primer surface; remove them as specified and sweep lightly before overcoating, and confirm the compatibility of the next coat with the zinc-rich primer together with the maximum overcoating interval.
What limits apply at low temperature?
Low temperature extends drying and curing times. Below the minimum application temperature of the product, application stops, or heating and insulation are applied as the technical data allows; curing is never accelerated by adding extra curing agent.
What matters for immersion service and tank or pipe internals?
Beyond corrosion performance, consider the medium and its temperature, whether cathodic disbondment resistance is needed, and the conditions for application and maintenance. Immersion areas generally carry stricter system and film thickness requirements than atmospheric exposure; the technical data governs.

Enquiries on Technical FAQ

  • System selection for Technical FAQ: structure type, service environment and area are sufficient for a coating system to be proposed.
  • Quantity and price for Technical FAQ: take-off from area and design dry film thickness, quoted against quantity.
  • Documents for Technical FAQ: TDS and SDS on request.